Polymer Property : Flexural Modulus = 290 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 290 GPa

@Temperature 23.0 °C
42100 ksi

@Temperature 73.4 °F
Hexcel® HexPly® 954-2A Curing Cyanate Resin, M60J Fiber
Information provided by HexCel