Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.058 GPa | 298.5 ksi | ASTM D790 |
Kolon KOCETAL® WR301 Wear Modified Acetal Resin Improved weather resistant grade suitable for out door use. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Flexural Modulus | 2.058 GPa | 298.5 ksi | ASTM D790 |
Kolon KOCETAL® WR301LO Wear Modified Acetal Resin Improved weather resistance and low odor of FA. Applications: Weather resistant products at closed space. Information provided by API-Kolon. |