Polymer Property : Flexural Modulus = 3.16 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.16 GPa
458 ksi
ASTM D790
PolyOne Geon™ Vinyl Rigid Molding MR900 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Modulus 3.16 GPa
458 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers MS 100 Styrene Methyl Methacrylate Copolymer
Description: Styrene Methyl Methacrylate CopolymerInformation provided by Network Polymers Inc.
Flexural Modulus 3.16 GPa
458 ksi
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data)
Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX..
Flexural Modulus 3.16 GPa
458 ksi
ASTM D790
Samsung Cheil Industries Starex® HF-5330S ASA, Unreinforced  (discontinued **)
Amorphous Styrene Acrylonitrile (SAN)Characteristics: Heat Resistant: Impact and Chemical Resistance, Surface GlossApplications: Oil Filter Case, Lubricant Can, Refrigerator and Hair Dryer Component..
Flexural Modulus 3.16 GPa
459 ksi
ASTM D790
Global GP-150 High Impact Polystyrene
High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys
Flexural Modulus 3.16 GPa
458 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KAL22XXC Acetal Copolymer
LNP* LUBRICOMP* KAL22XXC is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added feature of this material is: Wear Resistant.
Flexural Modulus 3.16 GPa
459 ksi
ASTM D790
Ensinger Tecaform™ UD Blue Ultra Detectable Acetal Copolymer (POM)
TECAFORM® UD Blue is an Ultra Detectable acetal copolymer designed specifically for applications in the food industry. High speed food production lines detect particulate matter in the food product..