Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.19 GPa | 463 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 3.19 GPa | 463 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87570 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 3.19 GPa | 463 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® BFL2010 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Flexural Modulus | 3.19 GPa | 463 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® BFL2010 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Flexural Modulus | 3.19 GPa | 463 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Lexan® BFL2010 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC with improved flow. Available in opaque colors. |
|||
Flexural Modulus | 3.19 GPa | 462 ksi | Tangent; ASTM D790 |
Plastics Group Polifil® M-20 20% Mica-Reinforced Polypropylene Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l.. |
|||
Flexural Modulus | 3.19 GPa | 463 ksi | ASTM D790 |
Entec Hyrene® PSCRY 1.5 General Purpose Polystyrene Available in North America Features: Crystal, High Heat Resistance, General Purpose, High Molecular WeightRoHS Compliant Form: Pellets Information provided by Entec |