Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.21 GPa | 466 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L0659 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Modulus | 3.21 GPa | 465 ksi | ASTM D790 |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Flexural Modulus | 3.21 GPa | 465 ksi | ASTM D790 |
Americas Styrenics STYRON® 665 High Heat Crystal Polystyrene Product CharacteristicsAdditive freeFood Contact CompliantTypical ApplicationsFilmInformation provided by AmericasStyrenics LLC. |
|||
Flexural Modulus | 3.21 GPa | 466 ksi | 2 mm/min; ISO 178 |
Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000 PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast me.. |