Polymer Property : Flexural Modulus = 3.299 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.299 GPa
478.5 ksi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0436T40L1 Talc Reinforced
Flexural Modulus 3.299 GPa
478.5 ksi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0336M30L Mica Reinforced
Flexural Modulus 3.299 GPa
478.5 ksi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0339W30L Wollastonite Reinforced