Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | ASTM D790 |
PTS SAN-82TR SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 3.43 GPa @Thickness 6.40 mm |
498 ksi @Thickness 0.252 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOL GP2200 PP+GF20% Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Flexural Modulus | 3.43 GPa @Thickness 3.20 mm |
498 ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
LG Chemical LUPOY GN2101FC PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame RetardanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemi.. |
|||
Flexural Modulus | 3.43 GPa | 498 ksi | 5 mm/min; ISO 178 |
Gromax BFG10-BN00N1 Nylon 6 10% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1000FV PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1000RV PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1000RV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1000V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in .. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100FV PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1100V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 1100V PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | 2mm/min; ASTM D790 |
Denka TX-400S Transparent Resin Polymer (MS resin) Methyl Methacrylate Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Modulus | 3.43 GPa | 497 ksi | chs 0.05 in/min; tangent; ASTM D790 |
Diamond Polymers SAN 280 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Modulus | 3.43 GPa | 498 ksi | 2.8mm/min; ASTM D790 |
Asia International Enterprise (Hong Kong) 60T4 Nylon 66, 20% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Flexural Modulus | 3.43 GPa | 498 ksi | ASTM D790 |
Samyang Triloy® S460G15 Polymer Alloy, Reinforced Excellent impact, formability and weather resistance.220 is a reinforced grade.Applications: LCD Panel Frame - for dimensional stabilityInformation provided by Samyang. |