Flexural Modulus 1.79 - 3.43 GPa
260 - 498 ksi
Average value: 2.87 GPa Grade Count:14
Overview of materials for Acrylic, Heat Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o..