Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.727 GPa | 540.5 ksi | ASTM D790 |
Global 120-PC-Natural Acrylonitrile Styrene, General Purpose Grade Description-transparent, natural, medium impact resistance, high hardness, high heat resistance, good chemical resistanceApplications-automotive, electrical parts, household goodsInformation provide.. |
|||
Flexural Modulus | 3.727 GPa | 540.5 ksi | ASTM D790 |
Global 121-PC-Blue Acrylonitrile Styrene, General Purpose Grade Description-transparent, blue, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistanceApplications-automotive, electrical parts, household goodsInform.. |