Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 30.3 GPa | 4390 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON OE008A PPS - Branched (Europe-Africa-Middle East) LNP* Stat-kon* OC-1008 is a compound based on PPS - Branched resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 30.3 GPa | 4400 ksi | ASTM D790 |
Techmer ES HiFill® PEEK CF40 HF 40% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: High FlowInformation provided by TP Composites, Inc. |