Polymer Property : Flexural Modulus = 31000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 214 GPa
31000 ksi
Specialty Materials Hy-Bor Boron/Graphite Hybrid Prepreg Tape
Boron & Graphite prepreg. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil..