Flexural Modulus 21.448 GPa
3110.8 ksi
ASTM D-790
PlastiComp Complet® LCF40 - PA66 Nylon 66, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% carbon fiber reinforcementInformation provided by PlastiComp, Inc.