Polymer Property : Flexural Modulus = 32.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 32.0 GPa
4640 ksi
ISO 178
Vyncolit Neopreg Kinel® SK4504 S12 Carbon Reinforced Molding Compound
Epoxy based molding compound long carbon fiber reinforced suited for demanding tribologic applications under dry running conditions, exposed to a wide range of temperatures (-100°C up to 150°C)...