Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.228 GPa | 33.1 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman 18BOA Polyethylene
(discontinued **) Polyethylene 18BOA is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic mold.. |
|||
Flexural Modulus | 0.228 GPa | 33.1 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman Voridian D4009-A Polyethylene
(discontinued **) Voridian polyethylene D4009-A is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on aut.. |
|||
Flexural Modulus | 0.228 GPa | 33.1 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman D4044A Polyethylene
(discontinued **) D4044-A is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic molding equipme.. |
|||
Flexural Modulus | 0.228 GPa | 33.1 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman Voridian D4053-A Polyethylene
(discontinued **) Voridian polyethylene D4053-A is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on aut.. |
|||
Flexural Modulus | 0.228 GPa | 33.1 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
Eastman Voridian E6838-010A Polyethylene
(discontinued **) Voridian polyethylene E6838-010A is a low density formulation with medium slip used for injection molding. It is an outstanding material for molding lids and other container closures because it pro.. |