Mechanical Properties Metric English Comments
Flexural Modulus 0.231 GPa
33.5 ksi
ASTM D790
Teknor Apex Telcar® TL EF-6155 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Flexural Modulus 0.231 GPa
33.5 ksi
ASTM D790
Teknor Apex Telcar® TL EF-6155 UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Flexural Modulus 0.231 GPa
33.5 ksi
ASTM D790
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low temperature impactAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..