Mechanical Properties Metric English Comments
Flexural Modulus 22.8 GPa

@Temperature 23.9 °C
3300 ksi

@Temperature 75.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® F-562 Phenolic Prepreg, 8HS Silica Reinforced
Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environm..
Flexural Modulus 22.8 GPa

@Temperature 23.9 °C
3300 ksi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D790
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 4581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Flexural Modulus 22.8 GPa
3300 ksi
ASTM D790
PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled  (disco
Information provided by PolyOne™ Corporation
Flexural Modulus 22.8 GPa
3300 ksi
ASTM D790
Techmer ES HiFill® PA6/6 GF60 HS UV BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi..
Flexural Modulus 22.8 GPa
3300 ksi
ASTM D790
Techmer ES HiFill® PA6/6 GF60 L BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackInformation provided by TP Com..
Flexural Modulus 22.8 GPa
3300 ksi
Shinil Chemical SHINCON PA66 Electro Conductive Polymer
SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's ..
Flexural Modulus 22.75 GPa
3300 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UCF26AS PPA
LNP* THERMOCOMP* UCF26AS is a compound based on Polyphthalamide resin containing 30% Carbon Fiber, 10% Glass Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive..
Flexural Modulus 22.75 GPa
3300 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP UCF26AS PPA (Asia Pacific)
LNP* Thermocomp* UCF26AS is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 22.8 GPa
3300 ksi
ASTM D790
Techmer ES HiFill® PA6/6 GF70 HS L BK 70% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 70% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N..