Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.32 GPa | 337 ksi | Tangent (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 808 C5WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 2.32 GPa | 337 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 2.32 GPa | 337 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |