Flexural Modulus 2.325 GPa
337.2 ksi
ASTM-D-790
BCC Products MB 3500 Urethane Fixture Board
MB 3500 is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly sha..