Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.345 GPa
340.1 ksi
ASTM D790
Lucent Polymers PC-1403 Polycarbonate, Extrusion/Blow Molding Grade
Medium FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 2.345 GPa
340.1 ksi
ASTM D790
Lucent Polymers PC-1403FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade
Medium FlowAdd "R" for Added ReleaseAdd "U" for UV StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 2.345 GPa
340.1 ksi
ASTM D 790
MRC Polymers NAXALOYâ„¢ 773 ABS + PC Alloy
Information provided by MRC Polymers Inc.
Flexural Modulus 2.345 GPa
340.1 ksi
tangent; chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 3501 Natural 1002 ESCR Injection Molding Grade, Environmental Stress Crack Resistant
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.345 GPa
340.1 ksi
tangent; chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 3501E Natural 1002 ESCR Extrusion Grade, Environmental Stress Crack Resistant
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.345 GPa
340.1 ksi
tangent; chs 0.05 in/min; ASTM D790
Diamond Polymers ABS 3501E-1300 Extrusion Grade, High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 2.345 GPa
340.1 ksi
ASTM D790
Ineos Nova 5100 High Impact Polystyrene  (discontinued **)
Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold..
Flexural Modulus 2.345 GPa
340.1 ksi
ASTM D790
Ineos Nova 5104 High Impact Polystyrene  (discontinued **)
Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold..
Flexural Modulus 2.345 GPa
340.1 ksi
ASTM D790
Lucent Polymers TPP-330 Polypropylene, 30% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.