Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.41 GPa | 349 ksi | ASTM-D-790 |
BCC Products EB 6200 Epoxy Tooling Board EB6200 is a “grain-free” elevated temperature epoxy modeling material known for its superior surface finish, dimensional stability and the ability to maintain tolerances even after being subjected.. |
|||
Flexural Modulus | 2.41 - 32.0 GPa | 349 - 4640 ksi | Average value: 16.6 GPa Grade Count:67 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |