Polymer Property : Flexural Modulus = 349.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.412 GPa

@Thickness 6.35 mm
349.8 ksi

@Thickness 0.250 in
tangent; chs 2.5 in/min; 100 mm SL; ASTM D790
Diamond Polymers ABSPC 7030-HES ABS/PC Injection Molding Grade, High Impact
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.