Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.245 GPa @Thickness 6.40 mm |
35.6 ksi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Flexural Modulus | 0.245 GPa @Thickness 6.40 mm |
35.6 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL ED1045D TPO, Thermoplastic Elastomer Description: Injection Molding, TPO, Thermoplastic Elastomer, Soft TouchApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 1333-86-4, 25087-34-7 and 14807-96-6Information provided.. |