Mechanical Properties Metric English Comments
Flexural Modulus 25.0 GPa
3630 ksi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of..
Flexural Modulus 25.0 GPa
3630 ksi
ISO 178
Hexion Bakelite™ PF 13 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, inorganically mica filled, heat resistance, good electrical properties, UL listed molding compound 0.75 mm/V-1 (NC), 3 mm/V-0, standardized molding compound.Application ar..
Flexural Modulus 25.0 GPa
3630 ksi
Lehmann & Voss LUVOCOM® 1105-8355 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Flexural Modulus 25.0 GPa
3630 ksi
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis..
Flexural Modulus 25.0 GPa
3630 ksi
Lehmann & Voss LUVOCOM® 20-0951 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Flexural Modulus 25.0 GPa
3630 ksi
Lehmann & Voss LUVOCOM® 20-7868 Polyphthalamide, with carbon fiber and glass fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
Flexural Modulus 25.0 GPa
3630 ksi
Lehmann & Voss LUVOCOM® 1105-7536 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Flexural Modulus 25.0 GPa
3630 ksi
ISO 178
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining..
Flexural Modulus 25.0 GPa
3630 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP LX08411 PEEK
LNP* THERMOCOMP* LX08411 is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added feature of this material is: Opaque.
Flexural Modulus 25.0 GPa
3630 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON RE008 PA 66
LNP* STAT-KON* RE008 is a compound based on Nylon 66 containing 40% Carbon Fiber. Characteristics of this grade include: Electrically Conductive.
Flexural Modulus 25.0 GPa
3630 ksi
ISO 178
Vyncolit X655 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask..
Flexural Modulus 25.0 GPa
3630 ksi
ISO 178
Vyncolit X655RB Glass Fiber and Mineral Filled Novolac Phenolic
Novolac resin based, glass fiber and mineral reinforced. Grade with superior stiffness, high dimensional stability and high wear resistance. Good chemical resistance against several fuels at elevate..