Mechanical Properties Metric English Comments
Flexural Modulus 2.5506 GPa
369.93 ksi
ASTM D790
E-Polymers TEKAPPO® JF6 Un-Reinforced Flame Retardant Heat Resistance M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Flexural Modulus 2.5506 GPa
369.93 ksi
ASTM D790
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..