Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.272 GPa | 39.5 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE D 4112 BLK Ash is 14%. The moisture content is 0.05%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.272 GPa | 39.5 ksi | ASTM D790 |
Teknor Apex Telcar® TL-1182A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |