Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.7468 GPa | 398.39 ksi | ASTM D790 |
E-Polymers TEKAFIN® PH40FR Flame Retardant Heat Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Flexural Modulus | 2.7468 GPa | 398.39 ksi | ASTM D790 |
E-Polymers TEKASTER® F101FR Un-Reinforced Flame Retardant PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |