Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.03 GPa | 585 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp AF002L ABS (Asia Pacific) LNP* Thermocomp* AF002L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC.. |
|||
Flexural Modulus | 4.03 GPa | 585 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp AF002L ABS LNP* Thermocomp* AF002L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC.. |
|||
Flexural Modulus | 4.03 GPa | 585 ksi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-530CD3 031 Polymer Alloy, Fiber Reinforced and PTFE Modified Main Characteristics: Dimensionally stable and rigid; Stress resistant; Extremely low wear to 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsIn.. |