Flexural Modulus 1.90 - 4.28 GPa
276 - 621 ksi
Average value: 2.94 GPa Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..