Polymer Property : Flexural Modulus = 4.313 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.313 GPa
625.5 ksi
Z; ASTM D790
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer
This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire..