Mechanical Properties Metric English Comments
Flexural Modulus 4.475 GPa
649.1 ksi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers Nemcon™ H PC DP111/X1 Polycarbonate
Polycarbonate-Thermally and electrically conducting grade with high HDT and improved processability.Information provided by Ovation Polymers