Mechanical Properties Metric English Comments
Flexural Modulus 4.602 GPa
667.5 ksi
chs 0.05 in/min; ASTM D790
Diamond Polymers NPP25-1503 GF30 30% Glass Filled Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.