Polymer Property : Flexural Modulus = 4.6107 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.6107 GPa
668.73 ksi
ASTM D790
E-Polymers TEKAMID® HG10L 10% Glass Fiber Reinforced High Impact PA/ABS Alloy
Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB..