Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.88 GPa | 708 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP HH0420A PA11 LNP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Flexural Modulus | 4.88 GPa | 708 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP HH0420A PA11 LNP* THERMOCOMP* HH0420A is a compound based on Nylon 11 containing proprietary fillers. Added features of this material are High Specific Gravity. |
|||
Flexural Modulus | 4.88 GPa | 708 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL FE1410PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1410PW resin is a blend of polyphenylene Oxide (PPO) and polystyrene (PS) resin that contains 10% glass reinforcement. The resin is suitable for injection molding. Noryl FE1410PW resin has .. |