Polymer Property : Flexural Modulus = 4.93 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.93 GPa
715 ksi
Tangent; ASTM D790
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black
Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 4.93 GPa
715 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CM4219 PC+ABS (Asia Pacific)
Flexural Modulus 4.93 GPa
715 ksi
ASTM D790
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Flexural Modulus 4.93 GPa

@Temperature 23.0 °C
715 ksi

@Temperature 73.4 °F
EN ISO 178
Ensinger TECASINT 4021 Polyimide, Black, 15% Graphite (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..