Mechanical Properties Metric English Comments
Flexural Modulus 2.800 GPa
406.1 ksi
ASTM D790
Ravago Manufacturing Americas Enviramid™ N2300HL BK Post Consumer Recycle Nylon 6
Heat Stabilized, Lubricated, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.
Flexural Modulus 2.800 GPa
406.1 ksi
ASTM D790
Ravago Manufacturing Americas Enviramid™ N2300HL BK/UV2 Post Consumer Recycle Nylon 6
Heat Stabilized, Lubricated, UV Stabilized, Black, and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago.