Flexural Modulus 0.288 GPa
41.8 ksi
Dow LDPE 779I Low Density Polyethylene
DOW LDPE 779I resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent rigidity. Typical applications include caps..