Mechanical Properties Metric English Comments
Flexural Modulus 0.293 GPa
42.5 ksi
1% secant; ASTM D790
ExxonMobil LL 6202 Injection Molding Resin  (discontinued **)
LL 6202 is a narrow molecular weight butene copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear..
Flexural Modulus 0.293 GPa
42.5 ksi
1% Secant; ASTM D790
Multibase Multi-Flex® A 8814 Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase