Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.9078 GPa | 421.74 ksi | ASTM D790 |
KKPC Kuhmo GP 125EI General Purpose GPPS Key features: For phonograph, good profile properties. Common Uses: CD-CASE, THIN-WALLGPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding proces.. |