Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.296 GPa | 43.0 ksi | ASTM D790 |
LyondellBasell Petrothene® NA345009 Low Density Polyethylene (Blow Molding) ApplicationsPETROTHENE NA 345-009 is a low density homopolymer resin designed for blow molding applications. Excellent clarity combined with strength and high stiffness makes NA 345-009 an ideal ch.. |