Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.068 GPa | 445.0 ksi | ASTM D790 |
Ineos Nova 2580 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistanceApplications: Cutlery, Consumer electronicsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the physical and optic.. |
|||
Flexural Modulus | 3.068 GPa | 445.0 ksi | ASTM D790 |
Ineos Nova 2510 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy.. |
|||
Flexural Modulus | 3.068 GPa | 445.0 ksi | ASTM D790 |
Ineos Nova 2511 General Purpose Crystal Polystyrene
(discontinued **) High speed molding, Improved crack resistance, USP Class VIApplications: Cutlery, Light louvers, RazorsExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phy.. |
|||
Flexural Modulus | 3.068 GPa | 445.0 ksi | ASTM D790 |
Ineos Nova 2581 General Purpose Crystal Polystyrene
(discontinued **) Good blending resin, Good balance of flow, strength and heat resistanceApplications: Consumer electronics, HousewaresExposure to gamma radiation in the 2.02-6.06 megarad range has no significant eff.. |