Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.08 GPa | 446 ksi | ASTM D790 |
Multibase Multi-Pro® 4012 X Platinum Polypropylene Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase |