Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 31.23 GPa | 4530 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp P1000P PA 6 (Asia Pacific) LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 31.23 GPa | 4530 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp P1000P PA 6 LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Americas region. |