Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.28 GPa | 476 ksi | ASTM D790 |
PolyOne Nymax™ GF 1010 14 Black 13 Polyamide 6 (Nylon 6) The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of .. |
|||
Flexural Modulus | 3.28 GPa | 476 ksi | |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Flexural Modulus | 3.28 GPa | 476 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Fittings 210(HR) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 3.28 GPa @Temperature 93.0 °C |
476 ksi @Temperature 199 °F |
ASTM Test |
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry) Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st.. |