Polymer Property : Flexural Modulus = 4905 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 33.82 GPa
4905 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP LC008EXQ PEEK
LNP* THERMOCOMP* LC008EXQ is a compound based on Polyetheretherketone containing 40% Carbon Fiber. Added features of this grade include: Electrically Conductive, Easy Molding.