Mechanical Properties Metric English Comments
Flexural Modulus 3.431 GPa
497.6 ksi
ASTM D790
LG Chemical IF870S PMMA, General Purpose Grade for Injection Molding
Highest flowability of all gradesFeatures: Excellent transparency and eleganceWeather resistance and chemical resistanceSurface hardness and coloring propertySuperior electrical resistance and mecha..