Polymer Property : Flexural Modulus = 499.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 3.447 GPa
499.9 ksi
XY; ASTM D790
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer
Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized..