Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.24 GPa | 760 ksi | Tangent; ASTM D790 |
RheTech Products GC30P105-08FA 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM D790 |
Polymer Resources NY6-G13 Nylon 6, 13% Glass Reinforced Nylon 6, 13% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM Data |
BASF Capron® HPN 9333G Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron HPN 9333G is a 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface a.. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | |
Fibre Glast 1110 L Vinyl Ester Resin (Laminate Properties) #1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista.. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2110 PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM D790 |
Techmer ES HiFill® PEI/C GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66 LNP* THERMOCOMP* RZ006S is a compound based on Nylon 66 resin containing 30% Milled Glass. Added feature of this material is: Heat Stabilized. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66 (Asia Pacific) LNP* Thermocomp* RZ006S is a compound based on Nylon 66 resin containing Milled Glass. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX4605 PPE+PS PPE+PS blend. 20% Glass reinforced. High heat. Dimensional stability. Suitable for automotive and E/E applications. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2110N PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2110R PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2110R PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem ATX102R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM D790 |
Ecomass® 1080CO94 Copper Powder Filled Polyamide Alloy, Injection Molding Moderate Specific Gravity, Copper Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing.. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM D790 |
Aaron Industries AAROPRENE® MFN 6001 Mineral Filled Nylon 6 AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM D790 |
Aaron Industries AAROPRENE® GFPC 5020 Glass Filled Polycarbonate AAROPRENE® GFPC 5000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS/PBT GF15 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM Data |
BASF Capron® HPN 9333G HS Impact Modified, 33% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron HPN 9333G HS is a heat stabilized, 33% glass reinforced, impact modified polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with.. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem 2110N PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 5.24 GPa | 760 ksi | ASTM D790 |
Techmer ES HiFill FR® PPO/HIPS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by Weight Appearance: BlackInformation provided by TP Composites, Inc. |