Flexural Modulus 2.41 - 5.40 GPa
350 - 783 ksi
Average value: 4.26 GPa Grade Count:7
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum..