Polymer Property : Flexural Modulus = 5.448 GPa
Polymer Property :
Flexural Modulus =
5.448 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
5.448
GPa
790.2
ksi
tangent; ASTM D790
Entec Hypro™ PPH-GF30 Natural Homopolymer Polypropylene, 30% Glass Reinforced
Information provided by Entec