Polymer Property : Flexural Modulus = 5.894 ksi
Polymer Property :
Flexural Modulus =
5.894 ksi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Flexural Modulus
0.04064
GPa
5.894
ksi
ASTM D790
Diamond Polymers Softflex® 1302 Thermoplastic Elastomer Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.